ABSTRACT

 

Degradation of Sudan I dye had been done with sonolysis and photolysis by adding anatase-TiO2.  Sonolysis method were performed using an ultrasound with frequency  of 45 kHz. Photolysis method were performed using an irradiation of UV light with λ = 359 nm.  Degradation of 4 mg/L Sudan I with addition of 0.1000 g anatase-TiO2 at pH = 7.0, temperature 25 ± 1°C, percentage of degradation 64.04% within 180 minutes sonolysis.  Degradation of 4 mg/L Sudan I using photolysis with addition of 0.1000 g anatase-TiO2 at pH = 7.0 and percentage of degradation 100% within 180 minutes photolysis. Degradation of 4 mg/L Sudan I using sonolysis and photolysis  simultaneously with addition of 0.1000 g anatase-TiO2 at pH = 7.0 and percentage of degradation 94.04% within 180 minutes treatment.  

 

Keywords : degradation, sonolysis, photolysis, Sudan I, anatase-TiO2.

References

Andayani, W., Sumartono, A., 1999, Aplikasi Radiasi Pengion Dalam Penguraian Limbah Industri, Radiolisis Larutan Standar Zat Warna Reaktif Cibarcon Violet 2R, Majalah Batan, Vol. XXXII No. 1/2.

Destaillats, H., Anderson, T. W., Hoffmann, M. R., 2001, Aplication of Ultrasound in NAPL Remediation Sonochemical Degradation of TCE in Aqueous Surfactant Solutions, J. Environ. Sci. Technol.,35: 3019-3024.

http://www.und.ac.za/und/org/sonochem. 5 Januari 2006).

http://www.KimiaUI.titania/2000/htm.Aktivitas Fotokatalitik pada Permukaan TiO2. (10 Januari 2006).

Stock, N. L., Peller, J., Vinadgopal, K., Kamat, P. V., 2000, Combinative Sonolysis and Photocatalysis for Textile Dye Degradation, J. Environ. Sci. Technology., 34: 1747-1750.

Hiskia, A., Ecke, M., Troupis, A., Kokorakis, A., Hennig, H., and Papaconstantnou, E., 2001, Sonolytic, Photolytic and Photocatalytic Decomposition of Atrazine in the Presence of Polyoxometalates, J. Environ. Sci. Techology., 35: 2358-2364.

http://en.Wikipedia.org/wiki/SudanI. (2 Januari 2006).

http://www.saujaya.com/sol_yel14.htm. (5 Januari 2006).

http://ntp.niehs.nih.gov/index.SUDANI. (2 Januari 2006).

http://ww.ncbi.nlm.nih.gov/entrez/query. (2 Januari 2006).

Arief, S., Safni, Roza, P. P., 2007, Degradasi Senyawa Rhodamin B Secara Sonolisis dengan Penambahan TiO2 Hasil Sintesa Melalui Proses Sol-Gel, J. Ris. Kim., 1(1): 64-70.

Peller, J., Wiest, O., Kamat, P. V., 2001, Sonolysis of 2,4-Dichlorophenoxyacetic Acid in Aqueous Solution. Evidence for ·OH- Radical-Mediated Degradation, J. Phys. Chem. A., 105: 3176-3181.

Basri, D., 2005, Degradasi Metilen Biru Secara Sonolisis dengan Penambahan TiO2-Anatase, Skripsi, Universitas Andalas.

Wang, J., Guo, B., Zhang, X., Zhang, Z., Han, J., and Wu, J., 2005, Sonocatalytic Degradation of Methyl Orange in the Presence of TiO2 Catalysts and Catalytic Activity Comparison of Rutile and Anatase, J. Ultrasonics Sonochemistry.,12: 331-337.

Khopkar, S. M., 1990, Konsep Dasar Kimia Analitik, UI Press, Jakarta, 201-227.

Safni, Zuki, Z., Haryati, C., 2008, Degradasi Zat Warna Alizarin S Secara Sonolisis dan Fotolisis Dengan Penambahan TiO2-anatase, J. Pilar, (submitted).

Downloads

Published

2015-02-12

How to Cite

-, S., Loekman, U., Febrianti, F., -, M., & Sakai, T. (2015). DEGRADASI ZAT WARNA SUDAN I SECARA SONOLISIS DAN FOTOLISIS DENGAN PENAMBAHAN TiO2-ANATASE. Jurnal Riset Kimia, 1(2), 163. https://doi.org/10.25077/jrk.v1i2.67

Issue

Section

Articles

Citation Check